Saturday, October 30, 2010

Re: [MW:7932] No of Welders

To my knowledge there is no limit for number of welder qualification  upon one WPS, You can qualify as many as per to the requirement for your project. 
 
 
 
Here By,
 
P.BalajiRajan,
-------Original Message-------
 
From: Arun Das
Date: 10/28/10 17:39:52
Subject: [MW:7911] No of Welders
 
Sir,
 
Minimum number of welders to be qualified upon one WPS is mentioned in SEC 1X or API 1104.
We are using PIPE,16"X0.375"WT STD SCH API 5L X52
 
Thanks in advance
 
with regards,
 
Arun S Das

 
FREE Animations for your email - by IncrediMail! Click Here!

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...