only a thin coating was allowed it does not say full painting system.

On Mon, Nov 30, 2009 at 6:39 PM, daniel iordache <daniel.iordache@gmail.com> wrote:
Hi, 

I have a strange situation about Hydrostatic Test ......

Until now we used to let all welds of piping system no painted........

now our client read in B31.3 and open the discussion that in code is wrote that is allowed to paint the welds before hydrostatic test......

What do you think about that?????

regards

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...