Re: [MW:3779] hydrotest b31.1

Yes code allowed hydrotest with painting. Only painting is not allowed for sensitive leak test as per B31.3.
 
Prsently in my site we are carried out hydro test in painted condition (around we did 2000 package in my site in painted condition)
 
Louis
Welding/Piping Inspector
Cswip 3.1 and API 570 Inspector
Singapore.

--- On Mon, 30/11/09, daniel iordache <daniel.iordache@gmail.com> wrote:

From: daniel iordache <daniel.iordache@gmail.com>
Subject: [MW:3771] hydrotest b31.1
To: materials-welding@googlegroups.com
Date: Monday, 30 November, 2009, 8:09 PM

Hi, 

I have a strange situation about Hydrostatic Test ......

Until now we used to let all welds of piping system no painted........

now our client read in B31.3 and open the discussion that in code is wrote that is allowed to paint the welds before hydrostatic test......

What do you think about that?????

regards

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone