[MW:3536] Re: acceptable tolerences in plumb and level in pipe

 
Right now I do not have the EIL spec no but I do have MECON Ltd's spec no which is exactly in line with EIL spec.Mecon std no is "MEC/SD/05/62/06/01"
Regards
Aarpee

On Wed, Oct 21, 2009 at 1:36 PM, PRAVEEN KUMAR <praveenkumar.sek@gmail.com> wrote:
Dear aarpee,
Thanks for ur info.
pls give me ASME stds  & EIL specifi.No
 
 
Regards,
Praveen


On Wed, Oct 21, 2009 at 11:58 AM, Ramprasad Chari <ramprasad.chari@gmail.com> wrote:
+/- 3mm on spool lengths and attachments
+/- 1.5mm lateral translation
+/- 1.5mm rotational
+/- 1.0 mm out of alignment
Above is as per Engineers India Ltd specs
Regards
Aarpee

On Wed, Oct 21, 2009 at 11:08 AM, Sadique Sheikh <sadiq.mech@gmail.com> wrote:

Good morning to all group member.
I would like to as that how much deviation is acceptable in pipe
alignment for plumb and levelness?
Can we confirm alignment with level guage only or it has some
tolerences from codes?
Plz give me detail with references.
Thanks in advance.
Regards
Sadique --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...