Skip to main content

[MW:3489] Re: WPS/PQR, Range Qualified

Prem,
You need impact test...? Why? The question can be answered as it is, see below yours.
It is a generic question. But still, I think a WPS is qualified to weld all if within its parameters. Imposition is on weld metal deposits (>12.5 mm per pass). WQT will decide what sizes a welder can weld.
SV

--- On Sun, 11/10/09, PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com> wrote:

From: PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com>
Subject: [MW:3482] Re: WPS/PQR, Range Qualified
To: raghurambathula@gmail.com
Cc: materials-welding@googlegroups.com
Date: Sunday, 11 October, 2009, 7:24 PM

Hi

What i interpret from the query is that the thickness of test coupon welded for PQR i.e while qualifying the WPS was 15mm.

Hence as per ASME SecIX, QW-451:which states the Procedure qualification thickness limits, the range of thickness "T" of base metal qualified will be 5mm to 30mm (2T).

Actually the question is not very clear and imp. details like impact requirements are missing ...

All are requested to pose clear,detailed to the point queries so that they can get correct answers / solutions.

Regards

Prem Nautiyal
Cell:9820313278

On Sun, 11 Oct 2009 14:06:21 +0530 wrote
>thickness limits are defined in QW 403.6 and 403.8, diameter is not a restriction for procedure but thickness limits are.to weld  20mm thickness your PQR test coupon thickness shall be at least 10mm
On Sun, Oct 11, 2009 at 10:53 AM, Shashank Vagal wrote:
Hi Group Members,Please see the following and advise.Shashank Vagal

Query:

dear every one,

i have this problem i need to know the thickness range or pipes diameter
range for the wps in which standard i think its in asme sec 9 but where ???

for exmple if i have wps for thickness 15 is it cover the 20 mm

waiting answer please

regards

My Reply:

 

A WPS is a guideline to ensure joint integrity as proven by
PQR + applicable mech tests + NDT. It is intended for all job sizes once the
welding technique used proves itself in these tests. The sizes etc come in to
picture by qualifying welder on test coupons of a given size as per your job
requirements. ASME IX stipulates weld metal deposit and not job size. Please
ref to QW 450 - 461.


Now, send attachments up to 25MB with Yahoo! India Mail. Learn how






PREM S NAUTIYAL
CELL : 9820313278




Keep up with people you care about with Yahoo! India Mail. Learn how
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...