Correct. Valves have (often) different leak classes. Those mentioned by Johnson Madakayil (class I, II,...V) is for control valves as per ANSI FCI 70-2.
 
On/off and check valves normally has the leakage rates specified in accordance with API 598, ISO 5208 or EN 12266-1. Here API 598 does not use leak classes. The ISO and the EN standard operates with leakage rates ranging from A (strongest requirement = zero leakage) to rate G weakest rate.
However, these leakage rates or classes are all for new valves being tested in the factory. After a valve has left the factory, it is probably not possible to have a valve to fulfil these factory acceptance tests. Valves that has been in use for some time may show much larger leakages than those specified/acceptance tested.
Regards
Kristian  


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Johnson Madukayil
Sent: 25. oktober 2009 14:56
To: materials-welding@googlegroups.com
Subject: [MW:3540] Re: 3534] RE: 3533] Re: 3531] Valve in hydrotest, is is allowed?

Valves have different leak classes. I think they go upto class V, with class V the most stringent. So even if the hydrotest is done, the valve may show some leak which could very well be within acceptable limits.

Regards

On Thu, Oct 22, 2009 at 3:05 AM, Kristian Lund Jepsen (KUJ) <KUJ@ramboll.com> wrote:
My experience with this problem is that the valve manufacturer need to be asked.
I recently had such a case, where the valve manufacturer accepted the test pressure, but the test-duration (30 minuttes for the piping in that case) could not be accepted by the valve manufacturer.
 
Therefore, in the end, we had to set a plug in the valve inlet, to avoid pressure testing against the valve closing mechanisms themselves.
 
regards
Kristian


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Rajneesh Gaur
Sent: 22. oktober 2009 08:28
To: materials-welding@googlegroups.com
Subject: [MW:3534] RE: 3533] Re: 3531] Valve in hydrotest, is is allowed?

Mr. Shashank,

I agree with Steven, but it’s still a possibility if the client insists to do it. Although in normal cases we do not prefer to do it.

Secondly as far as rating is concerned if a valve is designed to withstand certain pressure, it is expected to withstand the without leaking in closed position.

As far as seat testing is concerned seat has to be tested from one/both sided at the manufacturer’s facility either by pneumatic or hydro testing. This again depends on the type, size and rating of valves e.g. flow control valves can be tested from one side as per flow direction (marked on the valves).   

The decision I believe depends on of the criticality of the job, type of valve and its intended application and the most important the client’s requirement.

 

Regards

Rajneesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Steven Ko
Sent: Thursday, October 22, 2009 10:03 AM
To: materials-welding@googlegroups.com
Subject: [MW:3533] Re: 3531] Valve in hydrotest, is is allowed?

 

Hi Shashank,

 

All valves install in the system had a design pressure that can withstand the normal hydrotesting practise of 1.5 times of the operation pressure shall be acceptable without causing any damage to the valve. Full bore valve shall in the half open position to had the body tested as well during testing and the rest can be tested together in the system.

 

Closed valve in testing system used as isolator only tested one side of it and its not acceptable.

 

Seat testing of valves installed in the system pressure testing system its not appropriate as the flow of pressure need to determine which side to be tested and site testing its sometime hard to achieve this.

 

All seat testing normal tested by using low pressure air test on high pressure side and held for couple of minute, sometime its need to be tested on both ends depend on valve type. High pressure testing do employ but its depending on type of valves used and requirement..

On Thu, Oct 22, 2009 at 12:38 PM, Rajneesh Gaur <rajneeshgaur@gmail.com> wrote:

Mr. Shashank,

It will depend of the client requirements, and rating of the valve under consideration.

If the client asks for it to be done, it can be done provided the valve rating permits.

It would further prove the leak tightness of the valve or the quality of valve along with the line.

I have witnessed such hydro test.

 

Regards

Rajneesh

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal
Sent: Thursday, October 22, 2009 5:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:3531] Valve in hydrotest, is is allowed?

 

Hi,

Is it advisable to pressure test a water line for up to 10 bars with a valve already installed. (the valve will not be spaded during the test, it will only be in closed position)

 

Regards,

Shashank Vagal

 


Keep up with people you care about with Yahoo! India Mail. Learn how

 

 




--
Thanks you,

Best regards,
Steven Ko

email add:steven_ko@yahoo.com / stevenkmko@gmail.com




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...