[MW:3381] RE: 3376] Re: Electrode for LTCS A333Gr6

Hi,

 

For better achieving impact at -46 Deg.C, E 7016-1 (Root) + E7018-1(Hot, Fill and Cap) also recommended, since both are tested at -45 deg.C.

 

Note: Check your LAST requirement and choose the consumable accordingly.

 

Regards,

Vasanth


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of amarjit Singh
Sent: 29 September 2009 16:13
To: materials-welding@googlegroups.com
Subject: [MW:3376] Re: Electrode for LTCS A333Gr6

 

Dear Kaushik,

 

SA 333 Gr 6 is generally recommended upto -46 deg C so you can use E7010 for root pass & E7018-1 for filling & capping or for better control you can also use GTAW root

 

Amarjit singh

On Mon, Sep 28, 2009 at 5:58 PM, checks patel <checkspatel@gmail.com> wrote:

Dear All,

 

I have a U/G pipeline of ASTM A 333 Gr.6 (LTCS) for 2 KM.

 

Which Electrode I can use for root pass and other pass and with which techniqe.

 

 

Regards,

 

Kaushik

 




--
Amarjit Singh


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

Unknown said...

1.)SA 333 Gr 6 is generally recommended upto -46 deg C so you can use E80S NI1(SFA 5.28) FILLER WIRE(GTAW) for root pass & E7018-1 for filling & capping or for better control

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...