[MW:3353] Re: Heat Input


Adi ,

Pls refer to ASME Sec II C ,  where information about heat input depending upon the diameter & manufactures recommendation. In general client may restricted this parameter,

High Input leads to lower the toughness , ductility & increases the Hardness ,  if your value is accepted to client , no issue



Thanks & Best Regards,

Vinayak Kale
E & C  DIv. QA & I , OGSP
Larsen And Toubro Ltd
Powai , Mumbai
vinayak_kale@lntenc.com
Ph No.+91- 67053805/3685
Fax No. +91-67051988
(M) - + 91 9892743803



Adi <adinraos@gmail.com>
Sent by: materials-welding@googlegroups.com

09/29/2009 09:35 AM

Please respond to
materials-welding@googlegroups.com

To
"Materials & Welding" <materials-welding@googlegroups.com>
cc
Subject
[MW:3352] Heat Input







I have done the PQR for LTCS by using 6010 & 7018-1 as per ASME SEC IX
some time i got 5KJ heat in put
What is the limitation for heat input and where it is mention?

Adi




Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...