Dear Asad,

The acceptance of PT can't be used for visual defect as this is the acceptance for size of indication only not the size of the defect. 4mm indication may come from 1mm pin hole. It depends on the amount of dye contained by the defect which comes out from the defect (due to blotting action) when developer applied.

The size of defect you are refering may give you 15-20mm indiacation.

Regards.
CK

2009/9/28 asad azmi <azmiasadayub@gmail.com>
GOODMORNING...........
 
can anybody can confirm  whether a pin hole of diameter 3mm and depth of approximately 5 mm in fillet weld  of 6mm of material SA 516GR 70  can be VISUALLY accepted. The vessel is fabricated as per ASME SEC VIII DIV 1.
 
If YES then by which code.
 
Kindly note that if we consider acceptance crieteria  for PT/MT, as per ASME SEC VIII DIV 1, APPENDIX 6/8, Rounded indication upto 4.8mm is acceptable.
 
can the above defect can be accepted on the basis of acceptance crieteria of PT/MT.
 
 
please reply ASAP.
 
Thanks & Regards
 
Asad Azmi



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...