Dear Saravanan,
Test that pinholes by holyday, if they pass then no problem, if they don't check the mixture of components (including time, method and proportions of components)
Date: Sat, 26 Sep 2009 13:24:44 +0400
Subject: [MW:3325] Re: Painting
From: rajagopal.kannan@gmail.com
To: materials-welding@googlegroups.com
More than mailāWindows Live⢠goes way beyond your inbox. More than messages
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Test that pinholes by holyday, if they pass then no problem, if they don't check the mixture of components (including time, method and proportions of components)
Date: Sat, 26 Sep 2009 13:24:44 +0400
Subject: [MW:3325] Re: Painting
From: rajagopal.kannan@gmail.com
To: materials-welding@googlegroups.com
Dear saravanan,
To my knowledge I could visualize two problems based on similar past experience.
1. see the painting environment. was there any chance of mud or contaminants mixup.
2. thinner mixed may not be of appropriate proportion as per the data sheet.
Thanks and Regards,
K.Rajagopal
On Sat, Sep 26, 2009 at 12:46 PM, Saravanan Mohan <sardev@gmail.com> wrote:
Dear Guys!!!!!!!The project which I am involved following the paint systems as per client spec follows:-Inorganic Zinc(75-100 micron) as a primerHigh Build Epoxy(100-150 micron) as a IntermediateHigh Solid Aliphatic Polyurethane(40-100 micron) as a finishTotal Dft between (215-350 micron)After the complete curing of the finish coat visually I observed tiny pinholes like appearance or fish eye only inspector eye can find them.Please give me the suggestion where the problem from? this appear in almost all the painted works which applied many different days, different paint batch followed by airlesspray method.
More than mailāWindows Live⢠goes way beyond your inbox. More than messages
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments