Something to add to this GMAW discussion:
 
I've performed quality control work and inspection at a large piping fabrication shop where they were using mainly STT GMAW because of the high production rates inherant with this welding process.  There were mainy issues with lack of fusion or porosity in the root and the quality of welds being of concern.  I've later talked with welding engineers and consultants who have said that any type of GMAW process, whether its STT or other, will be susceptible to these types of defects, especially in the root of the weld. 
 
I'm not saying it's impossible to perform but the welders must have very good training with the capabilities of the machines and they must be aware of the difficulties in root welding otherwise you will have a large quality "headache" on your hands.  One possible solution is to grind away any weld starts that are suspect at having defects before welding over with the following passes (the welders at the shop I was working did not do this from what I could see and hence, likely propagated the problem).
 
Regards,
 
J.Z. 
Materials & Welding Engineer

--- On Thu, 9/24/09, Vishal Mehta <vdm@supertechservices.in> wrote:

From: Vishal Mehta <vdm@supertechservices.in>
Subject: [MW:3309] Re: application of SS Flux cored wire for GTAW, SFA 5.22
To: materials-welding@googlegroups.com
Received: Thursday, September 24, 2009, 9:24 PM

Yes, STT is a good option only if you could use GMAW process. And its worth an investment only if such jobs are regular.

Besides STT, even Miller Electric has developed their patented technology RMD - Regulated Metal Deposition. Machine Model is Pipepro 450. Its somewhat similar to STT and a little more to offer. check www.millerwelds.com

Regards

VISHAL



On Fri, Sep 25, 2009 at 8:54 AM, vipin george <vipingeorges@gmail.com> wrote:
Dear Bathula,
 
A new process is developed by Lincoln STT(Surface tension transfer) it's GMAW process with short circuit transfer.It's good for piping applications.Check Lincol electric.

Regards,
vipin


On Tue, Sep 22, 2009 at 12:57 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Dear members

We have typical vessel (site assembly), where backing gas arrangement could not be done for a stainless steel joint due to Safety (confined space), as well as space constraint.

One of the options will be using flux cored wire for GTAW.

Please share your view on these consumables for root pass of GTAW Stainless steel; where backing gas application is impractical, any body used these consumables?

Kobleco is manufacturing these wires under TGX series, any other manufactures who has similar product for this application?










--
SUPERTECH SERVICES LTD
Plot A-253, Road 30B,
Wagle Indl Estate,
Thane W 400 604
Maharashtra, India
Tel: +91-22-25826190/91
Fax: +91-22-25826189
Email: vdm@supertechservices.in
Web: www.supertechservices.in


Instant message from any web browser! Try the new Yahoo! Canada Messenger for the Web BETA --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...