[MW:3307] Re: application of SS Flux cored wire for GTAW, SFA 5.22

Dear Bathula,
 
A new process is developed by Lincoln STT(Surface tension transfer) it's GMAW process with short circuit transfer.It's good for piping applications.Check Lincol electric.

Regards,
vipin

On Tue, Sep 22, 2009 at 12:57 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Dear members

We have typical vessel (site assembly), where backing gas arrangement could not be done for a stainless steel joint due to Safety (confined space), as well as space constraint.

One of the options will be using flux cored wire for GTAW.

Please share your view on these consumables for root pass of GTAW Stainless steel; where backing gas application is impractical, any body used these consumables?

Kobleco is manufacturing these wires under TGX series, any other manufactures who has similar product for this application?






--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...