Dear Rajneesh,

As per ASME SEC VIII DIV-1,

For thickness above 6 mm "Hard stamp"to be used

For Thickness below 6 mm" Low stress stamp"to  be used

It's a good engineering practise to establish traceability.

Thanks & Regards,
vipin

On Thu, Sep 24, 2009 at 10:19 AM, Rajneesh Gaur <rajneeshgaur@gmail.com> wrote:

Dear all,

First of all I am new to the group and find the information very  interesting and useful.

Can someone answer this question, with references to code etc;

(1)  what is criteria of hard punch ?  when its required ? above what thickness it is allowed?

 

Regards

Rajneesh Gaur

 





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...