[MW:3304] Re: stamping on material

HI AL
most of clients refuse using the hard stamp specially for stainless steel materials, sometimes paint stencile is used.
go to ASME II SA 20 ( PARAGRAPH: MARKING ) TO SEE SOME LIMITATION FOR THE HARD STAMPING


BEST REGARDS...
QA/QC Eng./ Amr Soliman


--- On Thu, 9/24/09, Vinayak Kale <Vinayak_Kale@lntenc.com> wrote:

From: Vinayak Kale <Vinayak_Kale@lntenc.com>
Subject: [MW:3299] Re: stamping on material
To: materials-welding@googlegroups.com
Date: Thursday, September 24, 2009, 2:56 AM


Dear ,  Punching is only for the traceability & identification , few codes accept hard punching in terms of criticality & application criteria. impression marks must not in depth means should not affect thickness and should not create any undue stress

ASME VIII  Div 1 , Subsection A  - Part UG -  clause UG - 10 -General requirements -  enlighten more

Thanks & Best Regards,

Vinayak Kale
QA & I , OGSP
Larsen And Toubro Ltd
Powai , Mumbai
vinayak_kale@lntenc.com
Ph No.+91- 67053805/3685
Fax No. +91-67051988



"Rajneesh Gaur" <rajneeshgaur@gmail.com>
Sent by: materials-welding@googlegroups.com

09/24/2009 11:49 AM

Please respond to
materials-welding@googlegroups.com

To
<materials-welding@googlegroups.com>
cc

Subject
[MW:3298] stamping on material







Dear all,
First of all I am new to the group and find the information very  interesting and useful.
Can someone answer this question, with references to code etc;
(1)  what is criteria of hard punch ?  when its required ? above what thickness it is allowed?
 
Regards
Rajneesh Gaur
 





Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...