Dear Vinayak,

Thanks for your response.

 

Well this is what I found,

 

ASME B 31.1

133 STAMPING

Stamping, if used, shall be performed by a method

that will not result in sharp discontinuities. In no case

shall stamping infringe on the minimum wall thickness

or result in dimpling or denting of the material being

stamped.

CAUTIONARY NOTE: Detrimental effects can result from

stamping of material which will be in operation under long term

creep or creep fatigue conditions.

 

 Along with this we all know that the stamp should be low stress type with round edges of letters (sharp edges lead to stress concentration points on metal surface). It is generally not recommended for SS as it may lead to surface contamination. Etc.  The usage is dependent on criticality of fabrication (usage temp, cyclic conditions, loading, pr etc) . The questions I asked need specific documental references (if available) for solving the purpose.

I hope you/ someone can further enlighten on this topic.

Thanks in advance.

Regards

Rajneesh Gaur

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vinayak Kale
Sent: Thursday, September 24, 2009 10:57 AM
To: materials-welding@googlegroups.com
Subject: [MW:3299] Re: stamping on material
Importance: High

 


Dear ,  Punching is only for the traceability & identification , few codes accept hard punching in terms of criticality & application criteria. impression marks must not in depth means should not affect thickness and should not create any undue stress

ASME VIII  Div 1 , Subsection A  - Part UG -  clause UG - 10 -General requirements -  enlighten more

Thanks & Best Regards,

Vinayak Kale
QA & I , OGSP
Larsen And Toubro Ltd
Powai , Mumbai
vinayak_kale@lntenc.com
Ph No.+91- 67053805/3685
Fax No. +91-67051988


"Rajneesh Gaur" <rajneeshgaur@gmail.com>
Sent by: materials-welding@googlegroups.com

09/24/2009 11:49 AM

Please respond to
materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc

Subject

[MW:3298] stamping on material

 




Dear all,
First of all I am new to the group and find the information very  interesting and useful.
Can someone answer this question, with references to code etc;
(1)  what is criteria of hard punch ?  when its required ? above what thickness it is allowed?
 
Regards
Rajneesh Gaur
 





Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited </font


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...