Dear Ankit

In your case MDMT is -20 Deg C , For  Stainless steel ( SA 240 TP 316 L) impact test is not required as per UHA-51.



With Best Regards,

Rajeshkumar C Patel
Principle Engineer - Materials Technology, QA/QC & Standards


Linde Engineering India Pvt. Ltd.
'Linde House'
Opp: VUDA Office, VIP Road, Karelibaug,Vadodara - 390018, India.
Tel.: +91 265 3056706, Fax: +91 265 2335213 , Mobile:  +91 9909953459
Email : rajesh.patel@linde-le.com,


This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.





From:        Nandesh Kumar <nandeshkumar@rocketmail.com>
To:        materials-welding@googlegroups.com
Date:        03/11/2012 20:47
Subject:        Re: [MW:15846] requirment of Lateral expansion for P1 TO P8 PQR as ASME Sec IX
Sent by:        materials-welding@googlegroups.com





UHA-1 SCOPE
The rules in Part UHA are applicable to pressure vessels
and vessel parts that are constructed of high alloy
steel and shall be used in conjunction with the general
requirements in Subsection A, and with the specific
requirements in Subsection B that pertain to the method
of fabrication used.

Hence, the question originator has to mention the service applicable of the PQR in question.


Respectfully,

Nandesh Kumar A


--- On Sat, 3/11/12, Karthik <karthik6684@yahoo.com> wrote:


From: Karthik <karthik6684@yahoo.com>
Subject: Re: [MW:15845] requirment of Lateral expansion for P1 TO P8 PQR as ASME Sec IX
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Saturday, 3 November, 2012, 8:39 AM

Hi,
Please refer ASME Section - VIII,division 1 - UHA 51. According to that Lateral Expansion shall be reported on the Impact test report.

07     UHA-51        IMPACT TESTS
 

Impact tests, as prescribed in UHA-51(a), shall be per- formed on materials listed in Table UHA-23 for all combi- nations of materials and minimum design metal temperatures (MDMTs) except as exempted in UHA-51(d), (e), (f), (g), (h), or (i). Impact tests are not required where the maximum obtainable Charpy specimen has a width along the notch less than 0.099 in. (2.5 mm).
UHA-51(a) Required Impact Testing of Base Metal, Heat-Affected Zones, and Weld Metal
UHA-51(a)(1) Impact test shall be made from sets of three specimens. A set shall be tested from the base metal, a set shall be tested from the heat affected zone, and a set shall be tested from the weld metal. Specimens shall be subjected to the same thermal treatments1 as the part or vessel that the specimens represent. Test procedures, size, location, and orientation of the specimens shall be the same as required in UG-84.
UHA-51(a)(2) Each of the three specimens tested in each set shall have a lateral expansion opposite the notch not less than 0.015 in. (0.38 mm) for MDMTs of −320°F (−196°C) and warmer.


 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: Biplab Pal <biplab.mech@googlemail.com>
To:
materials-welding@googlegroups.com
Sent:
Saturday, November 3, 2012 11:30 AM
Subject:
Re: [MW:15841] requirment of Lateral expansion for P1 TO P8 PQR as ASME Sec IX


Dear Ankit,
 
In my opinion Lateral Expansion value is not mandatory for PQR.
If you see QW-170 of Sec IX, (for Charpy)
 
QW-170 NOTCH-TOUGHNESS TESTS
QW-171 Notch-Toughness Tests — Charpy V-Notch
QW-171.1 General.
Charpy V-notch impact tests shall be made when required by other Sections. Test procedures and apparatus shall conform to the requirements of SA-370.
QW-171.2 Acceptance.
The acceptance criteria shall be in accordance with that Section specifying impact requirements.
If you also go to the SA370 of Sec II part A column 27. (Records)
There is also nothing mensioned about Lateral Expansion.
It may me mandatory for checking the base material but not for PQR.
Anybody have other opinion please refer the code references.
 
 


On Thu, Nov 1, 2012 at 9:58 AM, Ankit PAtel <ankit.patel@orientalindia.net> wrote:
Dear Experts,
 
We have performed a PQR for 25 thk  plate , P1(SA 516 GR-70 ) To P8(SA 240 TP-316L). These PQR has been stress relieved at 620° C & impact tested at -20°C.
The testing laboratory has noted down only the joule values for the impact test, but they have not noted the Lateral Expansion Values P-8 Material.
The Avg. Joules Values observed are as follows:
Weld-72.67 J
HAZ(GR-70)-35.33J
HAZ(GR-316L)-158 J
PARENT(GR-70)-51.33J
PARENT(GR-316L)-298 J
 
Now our TPI says that for GR-316L Lateral Expansion Values is must for acceptance of the PQR.
Is it so?
Or based on these joules values these PQR can be accepted & used for weld having requirement of impact  test at -20°c
 
 
Thanks & Regards
Ankit Patel
Engineer Quality

 
 
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--

Thanks & Regards
Biplab Pal
Welding Inspector

E-mail:   biplab.mech@gmail.com

Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...