Dear All,
 
Greetings.
 
A vessel is being fabricated as per ASME SECTION VIII DIV 1.
 
a vessel requires PWHT becuase of the Service requirment.
 
Shell plate material is  SA537 CL1 - 36 mm thickness. maaterial is in NORAMALIZED Condition.
 
MTC is not highlighitng any PWHT( STRESS RELIEVING)  done for  the test coupons before conducting Mechanical testing.
 
My Question is  -  as vessel requires PWHT , how we will confirm the effect of PWHT on mechanical proerties for the base material without conducting PWHT on the test coupon of the shell plate before conducting Mechanical test.
 
Please give code reference.
 
Thanks & Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...