RE: [MW:8221] (NAS144M) equivalent of this material??

Dear Pradeep Sir,

                            Thank you so much as your suggestion always gets closer or almost matches the exact requirements not only for this query even for almost all queries. It always gets easier to go ahead with.

How ever we wrote to Client and yes they have asked us to go ahead with UNS 31254 Duplex Stainless steel grades. I just do not have any idea about the cost involvement in these grades of steel, But I am surprised by the client requirement of resisting with A105 Grades Flanges with 31254 Lining, we wanted to offer duplex forged materials but client is client.. The Casting for valve bodies selected is CF3MCuN.

Thank you once again.

===================
Bagesh Kumar

Seoul 135985

===================

 


From: pgoswami [mailto:pgoswami@quickclic.net]
Sent: Friday, November 12, 2010 2:00 AM
To: materials-welding@googlegroups.com; materials-welding@googlegroups.com
Cc: bagesh.kmr@gmail.com; bagesh.kmr@gmail.com
Subject: RE: [MW:8111] (NAS144M) equivalent of this material??

 

Dear Bagesh,

 

Some information for your reference.The original material NAS 144M is a S.S with higher Nickel and Mo with enhanced pitting corrosion resistance in high chlorine environment. 316L can not be a substitute for this alloy, just because the composition (18Cr-8Ni-2Mo) would not sustain long in high chlorine environment. During the manufacture of acrylic esters and other  products if chlorination is apart of the process then it would harm 316L seriously.

 

If  NAS 144M is difficult to procure then, Avesta 254SMO or Allegheny Ludlum AL-6XN, or NAS 254NM could be the nearest alternatives. These alloys may be 15-20% more expensive compared to NAS 144M, but are available as ASTM/ASME grades, which makes it easy to procure all round the world.

 

I would like to query the selection of  Hastelloy-C-276.This alloy is no doubt a good alloy in a very high chlorine environment, but it costs a fortune, both as raw material and  welding consumable. This alloy is recommended to fight dew point and high temperature  corrosion, Flue Gas Desulphurization Units, where the chlorine content could be easily in the range of 20000 ppm or more.

 

Between 1997-1999  I worked as Procurement, Welding and Inspection Q.C for an acrylic Acid/Ester project in S.E Asia. A Jump from Stainless to Hastelloy is easily recommended by suppliers, especially, for control valves, measuring devices and many other items,however the cost of change of material may be prohibitive.

 

I would say, take a rationale look at the material selection and for the said environment, assess the corrosion rates for each material, service life of the plant then make your final selection. If you require, take the help of metallurgists or welding personnel well versed with these materials.

 

Thanks.

 

 

Pradip Goswami,P.Eng.,IWE

Welding & Metallurgical Specialist & Consultant

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bagesh
Sent: Saturday, November 06, 2010 8:12 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:8111] (NAS144M) equivalent of this material??

Thank you all for your inputs,

 We have written a technical clarification to client about the details and knowhow reason for the use of this material against the said service, however we have decided to go with the Hastelloy C276 for these services.

We have also contacted Nihon Yakin of Japan, but presumably they have obsolete this alloy and are offering higher grade equivalent to Hastelloy C276..

Will put the same when I receive  the inputs from the Vendor and client.

Thank you once again.

 

===================
Bagesh Kumar
Seoul 135985
===================

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Stefan SAUCIUR
Sent: Friday, November 05, 2010 11:23 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:8098] (NAS144M) equivalent of this material??

 

Please find this on

 

 

Best regards,

Stefan

--- On Fri, 11/5/10, Harish Kannepalli <harishkannepalli@gmail.com> wrote:


From: Harish Kannepalli <harishkannepalli@gmail.com>
Subject: Re: [MW:8086] (NAS144M) equivalent of this material??
To: materials-welding@googlegroups.com
Date: Friday, November 5, 2010, 12:57 PM

Dear Mr. Bagesh,

                           Thank you for introducing some new material to me as well as group. This material is a patented one almost equivalent to 316L. Please find the link attached for further info.

http://ip.com/pdf/patent/US6966973.pdf

2010/11/5 Bagesh <bagesh.kmr@gmail.com>

Hello there,

                  I have been doing a project in Korean peninsula and certainly while browsing through the piping material specification I have found NAS144M material and it has been used for the service of ACRYLIC ACID, REACTED GAS and ESTERS. The P T Rating for these services is 150 Rating.

When enquired with vendors they dont have any clue until we supply the correct material property, the contract MSD has shown 254SMO as the property of this material,

For the reference we have used SS316L for such services in other projects, but the client have rejected our request and they just resist on the material property,

Could any one have some brief on the said subject or equivalent ASTM spec or Its UNS no..

I do not have any other things to share on the same.

Regards

===================
Bagesh Kumar

Seoul 135985

===================

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--

regards,

Harish.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...