hello
what will be the thickness limit for welder, if i go for as below
1. carbon steel plate 14 mm thickness (P. No. 1 // G. No. 2)
2. coupon to be heat treated above upper transformation temp. say around 900 deg. C.
3. charpy impact test not required.
4. only SMAW process to be conducted.
5. single 'V" joint.
Can any gentleman send me a copy of WPS-WPQ-PQR set for reference.
ajay
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
what will be the thickness limit for welder, if i go for as below
1. carbon steel plate 14 mm thickness (P. No. 1 // G. No. 2)
2. coupon to be heat treated above upper transformation temp. say around 900 deg. C.
3. charpy impact test not required.
4. only SMAW process to be conducted.
5. single 'V" joint.
Can any gentleman send me a copy of WPS-WPQ-PQR set for reference.
ajay
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments