Larry

 

One treats cast steel similar to wrought steel. Match the strength of the cast steel with the strength of the electrode. Depending on carbon equivalent pre and post weld heating might apply.

 

If you have the grade of material I can be more specific.

 

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Larry
Sent: 01 October 2010 04:23 AM
To: materials-welding@googlegroups.com
Subject: [MW:7290] Electrode for cast steel

 

Hi,

 

Can anybody suggest a good electrode for cast steel?

 

No code applies, just common welding.

 

 

Thanks in advance.

 

 

 

Cheers,

Larry

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...