On Mon, Sep 14, 2009 at 7:13 PM, John Henning <jhenning@deltak.com> wrote:
weldable casting (carbon steel) grade B
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of saqib gul
Sent: Sunday, September 13, 2009 11:36 PM
To: materials-welding@googlegroups.com
Subject: [MW:3193] Valves A-216 WCB
We use valves specification e.g.Gate valve, cast steel, ASTM A-216 Grade WCB, Class 150, Flanged ANSI B 16.34My question is what does "WCB" stands for? If it is a grade of A-216 but what does it exactly mean? If some one know it's abbreviation?
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---