Hi Prakash,
 
Since the operation temperature its no high enough to remove the surrounding moisture and believe that its in operation now. The easy way it to had the bolts replace one after another with insulating gasket while reusing the bolts, remember to cleaning the contamination surface or apply with high temp grease over all bolts/( sealing off O2) and wrap around flangs connection with glass fibre tape saturated with the grease.
 
Do hope its help.
 
Rgds,
STV

On Sun, Sep 6, 2009 at 3:30 PM, prakash kamathuru <prakashkbp@gmail.com> wrote:
Hi Steven,
 
heat exchnger design tempr is
 
Tube side : -104/65 Deg C.
Shell side : 110 Deg C.
 
Now already at site bolt is getting corroded.So i want to prapose Client a PTFE coating option.Is it Okay according to procedure.If it is okay please give me some back up documents.
 
If you are giving me the useful hints with back up,very helpful for convincing client.
 
Regards,
Prakash K B.

On Thu, Sep 3, 2009 at 9:34 PM, Steven Ko <stevenkmko@gmail.com> wrote:
Hi Prakash,
 
Since this its heat exchanger, the operating heat will dry up any moisture around the vicinity and the galvanic effect will keep to the minimum. We had used  alot of this similar bolting in the offshore environment.
 
Rgds,
STV

On Thu, Sep 3, 2009 at 6:37 PM, mohan q8 <mohanq8@gmail.com> wrote:
Hi Nilesh,
 
How you can cote an fasteners using FBE coating? U need to re open the exchanger during maintanence or leakage pupose.
 
We need to know the the exchanger design perameters to deside on coating requirements, if it is working in normal atmospheric temperature we can cote with fluropolymer coating but this coating is generaly doing by manufacturer field application to be veriifed with manufacutere only.
 
If the exchanger working in high temperature we can coat with high temp silicone paints.
 
Regards
 
Mohan q8.

 
On Mon, Aug 31, 2009 at 12:45 PM, Nilesh Pathare <patharenil@gmail.com> wrote:
You can go for FBE ( Fusion Bonded Epoxy) coating for those bolts.
FBE coating is a good option. But check other parameters and the fluid if its affect the FBE material.

Regards,
Nilesh Pathare.



On Fri, Aug 28, 2009 at 2:48 PM, prakash kamathuru <prakashkbp@gmail.com> wrote:
Dear all,
 
Can any one help me to find the coating material for A320 Gr L7 bolts and A 194 Gr 2 nuts on SS 304 Flanges.As i checked the galvonic series Zn/mg not recomnded.Presently this heat exchnger flange which is already installed at site.Any Solution,so that without disturbing the joint we can coat some material at site for controlling galvonic corrosion.
 
Please keep in mind that it is STHE body flange.
 
Your feedbacks very helpful for me in taking decision and appriciated.
 
Regards,
 
Prakash





--
Best Regards,

Nilesh Pathare








--
Thanks you,

Best regards,
Steven Ko

email add:steven_ko@yahoo.com / stevenkmko@gmail.com










--
Thanks you,

Best regards,
Steven Ko

email add:steven_ko@yahoo.com / stevenkmko@gmail.com


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---