Hi Nilesh,
 
How you can cote an fasteners using FBE coating? U need to re open the exchanger during maintanence or leakage pupose.
 
We need to know the the exchanger design perameters to deside on coating requirements, if it is working in normal atmospheric temperature we can cote with fluropolymer coating but this coating is generaly doing by manufacturer field application to be veriifed with manufacutere only.
 
If the exchanger working in high temperature we can coat with high temp silicone paints.
 
Regards
 
Mohan q8.

 
On Mon, Aug 31, 2009 at 12:45 PM, Nilesh Pathare <patharenil@gmail.com> wrote:
You can go for FBE ( Fusion Bonded Epoxy) coating for those bolts.
FBE coating is a good option. But check other parameters and the fluid if its affect the FBE material.

Regards,
Nilesh Pathare.



On Fri, Aug 28, 2009 at 2:48 PM, prakash kamathuru <prakashkbp@gmail.com> wrote:
Dear all,
 
Can any one help me to find the coating material for A320 Gr L7 bolts and A 194 Gr 2 nuts on SS 304 Flanges.As i checked the galvonic series Zn/mg not recomnded.Presently this heat exchnger flange which is already installed at site.Any Solution,so that without disturbing the joint we can coat some material at site for controlling galvonic corrosion.
 
Please keep in mind that it is STHE body flange.
 
Your feedbacks very helpful for me in taking decision and appriciated.
 
Regards,
 
Prakash





--
Best Regards,

Nilesh Pathare




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...