Re: [MW:35288] Welding consumable for S355J2WP material

ER80S-Ni1(a nickel alloy filler wire), E81T1-Ni1C 9 (for FCAW process with 80 A+20 CO2) 
Please read it as "ER80S-Ni1(a nickel alloy filler wire), E81T1-Ni1C (for FCAW process with 
80 A+20 CO2)".
You can also try with E/ER309L which will help to avoid preheating or post weld cooing. But it 
is only an option.
Sridhar.


On Thu, 19 Sept 2024 at 19:27, sridhar cn <sridharcn305@gmail.com> wrote:
Mr.Xun Thong,
S355J2WP is a weathering steel.  E7018-1, E 8018-W2 (for higher strenths),
ER80S-Ni1(a nickel alloy filler wire), E81T1-Ni1C 9 (for FCAW process with 80 A+20 CO2) 
are generally suitable. 
Preheat & PWHT may be necessary to prevent cracking.
rgds,
Sridhar.

On Wed, 18 Sept 2024 at 21:22, Xuân Thông <xuanthong.hp@gmail.com> wrote:
Hi Experts,
Any one please give me the suggestion for welding consumables that will be used for S355J2WP.  If you have any WPS for this material, please let me know.
Thanks !

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-O%3DA4OKzV%2B%3DRPnGBKXVW5o_q0B5dT60Ftz_xB%2BWJNqDf1w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYii2jJYt43s0RPm5xypt8tnEra_rkJC-f3iJXg7nAmEq3A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...