Not advisable due to lower critical temp of CS is around 725 celsius whereas PWHT heat treatment temp for 91 is around 745 to 760 which will affect the properties of CS
Go with Mr Keskar recomondation.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Mon, Sep 16, 2024 at 1:07āÆPM Vijay Kumar <vijaytuty@gmail.com> wrote:
Dear Experts,I need SA335 P91 to SA106Gr.B Dissimilar Material Welding Procedure with some reference codes.Please shareThanksVijayakumar+91 8238450968--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be7e26e6-2446-4b69-8ed4-d10c5a074dcfn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMMBtYbvJ3x%3DDwhJgDmz8h2-%3DKVPH69kgG%2BgEJjVKZL9Q%40mail.gmail.com.
Comments