Friday, September 20, 2024

Re: [MW:35272] Hardness limit of SS 316L material

Please follow NACE MR0175

Regards,

On Mon, Sep 16, 2024 at 12:31 PM kumar sumit <kumarsumities@gmail.com> wrote:
Sir is there any reference standard plz quote. 

On Mon, 16 Sep, 2024, 11:55 am Macario Jr. Palola, <macario.palola@gmec.ph> wrote:
The hardness value of 316L stainless steel typically falls within the range of:

- Rockwell Hardness (HRB): 70-90
- Brinell Hardness (HB): Approximately 150-220

These values can vary based on the specific processing and treatment the steel has undergone.

On Mon, Sep 16, 2024 at 4:40 PM kumar sumit <kumarsumities@gmail.com> wrote:
Dear expert, 
                      Can anyone explain hardness limit(value) of P-8(TP316,SS316L). 

Eg:- as you know that hardness vale of CS is 200BHN.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACCHnjVGd7tiR8kA0-_G5y75nSwsN-2V%2BCECQHkmbKncBRafkg%40mail.gmail.com.

The information contained in this email is intended for use only by the recipient to whom or which this is addressed. Such information may be privileged, confidential, and/or proprietary subject to the GMEC Email Disclaimer. Moreover, as we value your privacy, we will handle and safeguard any personal data we receive in this email in accordance with our Privacy Notice.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFizHVWm5sf43wz5agDufcn32hDu1MR3VjOEHJ9ZYwuoVpDSEg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACCHnjW%3DzEKhu0sH88%2BtozsKuVOwpu_6B314_mvoU7qMJMVjSA%40mail.gmail.com.


--
Thanks & Regards,
 
Srinivasrao.Gundala,

Please consider your environmental responsibility: before printing this e-mail, ask yourself whether you need a hard copy!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACn7QWXzbpapxCQ9jPMXeEatFdFHXEmkcZGUpFiVbPdFtztORw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...