Re: [MW:35260] parent mental is 25crmo4 to 25crmo4. Is 80S-B2 filler material is suitable or anything else one plz suggest

Pl send details of mechanical and chemical properties of the base metal - 25 CrMo4
Pl detail out service conditions of components being fabricated 
Any specific application?
Thanks 
Vishwas - IWE 

9823472273
Sent from my iPhone

On 15 Sep 2024, at 3:34 PM, Mehul Patel <vmgmehul@gmail.com> wrote:

Dear Experts'


Plz suggest me filler metal for 25crmo4 & explain 80S-B2. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/168bfb14-9d86-4c3a-84d5-45ad0c8f4224n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...