Re: [MW:35251] in socket weld gap should be 1.5mm to 3mm and radiography should be 10% is it mention in b31.3 or not?

Dear Sir,

According to B31.3 -2020.

Clause 311.2.2 - Socket Welds (b) (2) - Weld dimensions shall not be less than shown in figures 328.5.2B and 328.5.2C.

Clause 341.4.3 (b) - Socket welds and branch connection welds that are not radiographed shall be examined by magnetic particle or liquid penetrant methods in accordance with para. 344.3 or 344.4.

Regards,
Deepanshu
Chartered Engineer - M1801486
ASQ Senior Member - 6600682
ASME Member - 000103695251
+91-7206362125


On Thu, Sep 12, 2024 at 10:40 PM Mohd Yasoob Azeem <yasoobazeem786@gmail.com> wrote:
Dear friend,

Greeting!

in socket weld gap should be 1.5mm to 3mm and radiography should be 10% is it mention in b31.3 or not?

Is this thing mentioned in ASME B31.3 or not?

I shall be very thankful for this kindness.


-- 
"Thanks & regards"
Mohd Yasoob Azeem

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9ba85e7e-9f73-49db-939d-345bea3bc75dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFvWzAzDknnarb%2BVvtx-4YFRZ0H8APfj0P-tEFNCrJdgAZjstw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...