Re: [MW:35251] in socket weld gap should be 1.5mm to 3mm and radiography should be 10% is it mention in b31.3 or not?

Gap 1.5 mm is addressed .
RT is not addressed
Sent from my iPhone

On 12 Sep 2024, at 8:10 PM, Mohd Yasoob Azeem <yasoobazeem786@gmail.com> wrote:

Dear friend,

Greeting!

in socket weld gap should be 1.5mm to 3mm and radiography should be 10% is it mention in b31.3 or not?

Is this thing mentioned in ASME B31.3 or not?

I shall be very thankful for this kindness.

-- 
"Thanks & regards"
Mohd Yasoob Azeem

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9ba85e7e-9f73-49db-939d-345bea3bc75dn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...