Re: [MW:35236] Overlay welding defects

Dear sir,

Welding Valve body & Adapter,(Ball Valve,Triple offset Butterfly,Trunnion mounted Ball Valve & Top Entry Ball Valve.


Regards,
R.Gowtham.

On Fri, Sep 6, 2024 at 11:21 AM Mohd Siraj <mohd52100@gmail.com> wrote:
WCB/LCB fitting elbow or tee components, pl follow,

weld with CS filler wire first then start overlay.

On Thursday, September 5, 2024 at 11:07:20 AM UTC+3 Karthick Flow Controls wrote:


Inconel 625 & 316L -GMAW
Shielding Gas - Argon 
Position -1G


Regards,
R.Gowtham.

On Wed, Sep 4, 2024 at 4:08 PM 'J Prinsen' via Materials & Welding <material...@googlegroups.com> wrote:
First questions: which process, which shielding gas, which welding position, which welding parameters

Regards

Jurgen Prinsen IWE
Weld-Tech BV
Welding Engineering and Consultancy


Van: "Karthick Flow Controls" <kfcco...@gmail.com>
Aan: "Materials & Welding" <material...@googlegroups.com>
Verzonden: Woensdag 4 september 2024 07:26:39
Onderwerp: [MW:35217] Overlay welding defects

Dear Experts,
Welding Overlay, After Machining the Pin holes and blow holes noticed in Overlapping Joint area, After attend the defects, It will open some other places, The defects noticed Uniform inline.   ( Overlay Material ,316L ,Inconel 625 ,St6 & ST21,Base Material WCB/LCB),
How to prevent the defects?




Regards,
R.Gowtham.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33a4e532-e9d1-45f0-a35f-2172b2263b12n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


--

Thanks & Regards,
R.GOWTHAM.
KARTHICK FLOW CONTROLS, 
1/575 SNMV College Road, 
Mallumichampatti,
Coimbatore - 641 050.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/287ab92f-439c-461a-9c0d-6a9c21ca53abn%40googlegroups.com.


--

Thanks & Regards,
R.GOWTHAM.
KARTHICK FLOW CONTROLS, 
1/575 SNMV College Road, 
Mallumichampatti,
Coimbatore - 641 050.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADsiqoGENtjXWAmz5FGB0JFFwQN0GAQ%3Dk9385JFQ-J7cn920tg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...