Tuesday, September 10, 2024

Re: [MW:35201] Filler wire for 321H

you may not get 347 /321 with minimum 0.04 % C
 u will get commercial grade of 0.08 %C maximum, if u required, Ask supplier to give with minimum 0.04 C.   It is not possible with base metal carbon content of 0.04 to 0.1C which is high carbon for application high temp service. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Aug 29, 2024 at 4:01 PM Vignesh Manoharan <vkemano@gmail.com> wrote:
Hi sirs,

Client not accepting 347 filler wire to Welding 321H.

Carbon content shall min 0.04℅.


Could you provide suggestion



Regards,
Vignesh M




On Sat, 24 Aug, 2024, 9:54 am Raviraj Gohil, <raviraj.gohil@lloyds.in> wrote:
You may use ER 347 GTAW filler wire

Thanks & Regards,

 

Raviraj Gohil | Manager - Welding | + 83473 02025 | www.lloydsengg.in 




On Fri, Aug 23, 2024 at 8:07 AM Vignesh Manoharan <vkemano@gmail.com> wrote:
Hi experts, 

What filler wire is required to weld 321H in GTAW process. ? 

Pls suggest


Regards
Vignesh M

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUncPL9Nh0PigpmvCq8YDrd%2B2SQsikfyt6_q0_ZU2RZ-aC7jg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BN2U4MfJgpQdHmY6S4-7DOpqUD0Jd_qKB3jAK-BYAGVO8L-5Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUncP%2BGbVoAqE99r%2BY0o1MZ_X2uizbcwMB%3DBYLMoSiaMrDhDA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMs%3DoVqxJtaS%3Dezhn9aRZ-mVHgN-EAP%2BMQTHOCtBoAauw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...