Re: [MW:35199] Clarification on Subsize Impact Specimens for PQR According to API 650

Try ASME Sec. IIA SA-370


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Thursday 29 August, 2024 at 12:38:55 pm IST, Binto George <bintogeorgev@gmail.com> wrote:


 Dear Experts?

We obtained a value of 26J(avg) for P1 G2 material during procedure qualification with impact requirements, whereas the acceptance criteria according to API 9.2.2.5 is 27J(Avg). We used a subsize specimen of 7.5 x 10 mm. Is there any relaxation or allowance for subsize specimens in this context? If so, where can I find this information?  

Regards,
Binto George

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f710ebaa-6272-48a0-a50f-969b22b0c818n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1427709181.702666.1724926231074%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...