Re: [MW:33592] PAUT Instead of RT

Dear Sir,

Thanks for sharing the information.

This job will undergo RN1, SR1 & SR2 - Generally which stage will do the PAUT, No any information from client.

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message


On Wed, Oct 12, 2022 at 7:32 AM srinivas rao <engr.srini@gmail.com> wrote:
PAUT can be used in place of  RT and allowed as per ASME SEC VIII DIV 1, check your weld quality before jumping to this mecthod and it is  better than RT and with more precision to detect defects. However  you need check with your NDT crew or your NDT sub contractors are they having compitent personal to perfrom  it is very important that the person who is  perfrom this shall be skilled enoughed to operate machines for  performing & interpreting results and all the welds in the vessel cannot have sufficient space on either side of the welds for scanning and hence interpretation of results may be difficult in case proper calibration and validation blocks are not place.

please refer ASME Code cases that are allowing  PAUT  in the lieu of RT 

you require to demostrate  PAUT mock up prior to NDE test to your client and AI. no of blocks will differ based on your scope take opion of your LEVEL III.

Thanks 
Rao
On Tuesday, October 11, 2022 at 2:37:32 PM UTC+4 anthony...@gmail.com wrote:
Yes it can be done

On Tue, 11 Oct 2022, 11:50 williams p wilson, <william...@gmail.com> wrote:
Dear Experts,

Please guide, RT can be replaced with PAUT for a vessel constructed with ASME Section VIII Div.1, MOC : SA 516 Gr.70, 70 / 80 mm Thickness.

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ5hNvmec_a_qxOBGp66-DVsdUR7mT3WHOvS-%3DKX_dq4vg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/efb6a491-23fc-430b-93df-b43510f270e3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7uweSkyQw3wm5UzY%3Da-g%3DCtXiUDA1Oehkx2Q8a%3D2-FqQ%40mail.gmail.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...