Dear sourav sir

      I have checked in Mandatory App. 2 Table II-200-I for SA-516 Edition 2019 is identical with ASTM-17 and other acceptable editions are 86 thru 17 and    
       SA-516 Edition 2021 is identical with ASTM-17 and other acceptable editions are 86 thru 17 (No change in Edition 2019 & 2021). However 2019 edition is
       out of range as per table-II-200-I  because Edition 2019 is equivalent to edition 2017 & Edition 2021 is also equivalent to 2017 base on that can we accept 
       the material  simply by mentioning that SA-516 Gr.70 Ed.2019 is equivalent SA-516 Gr.70 Edition 2017 also SA-516 Gr.70 Ed.2021 is equivalent SA-516 Gr.70
        Edition 2017 hence this is acceptable  or what else should be done in order to carry out the recertification please provide your guidance in this regard.

On Friday, October 7, 2022 at 2:52:55 PM UTC+5:30 sourav sharma wrote:
simply
first of all refer signed and approved QC manual ,refer material section .
For easy understanding refer below procedure-
Read  and refer ASME sec VIII div1 UG-10 for recertification 
1.first check that  ASME specification  Identical with  which ASTM Specification (eg in edition 2019 SA516 is identical which ASTM specification/year). check this in ed2019 only.
2.second check Identical  ASTM Specification is in range or not of acceptable editions  (Table II-200-1) ASME Sec II part A ed2021..check this in ed 2021.
3.Third if  Identical  ASTM Specification is in range of acceptable editions. simply stamp of recertification( ASME spec with editions spec with edition, date, sign, QA/QC engineer name and signature)
4. if  Identical  ASTM Specification is not in range of acceptable editions than make a table compare mechanical prop, chemical prop, heat treatment ,ASTM year of edition , grain type, number of mechanical test, orientation of specimen include all points given in certification of related specification and general specification(eg for SA516- refer SA 516 and SA 20 certification).
5.Write a note at end recertification done by following ASME sec VIII div 1 -UG-10 edition 2021.
6.Attach marking photos.
result- IF 2019 Edition values for mechanical prop, chemical prop and all other property satisfy need of edition 2021 use material by attaching all supporting docx-MTC,MIR,UG-10form.
IF 2019 Edition values for mechanical prop, chemical prop and all other property DIDNT satisfy need of edition 2021 have a words with AI go for testing and but testing will be useful only when chemical and heat treatment is as per req of 2021.

This is general procedure best to refer QC manual.

regards
sourav


On Fri, 7 Oct 2022 at 13:01, Saurabh Joshi <saurab...@gmail.com> wrote:
Dear All ,

     We have to manufacture a Heat ex-changer Code of construction ASME 2021(Code stamp required for the Equipment) . Raw material for plates & pipes are manufactured As per ASME 2019 . MTCs are available as per ASME 2019 and Original marking is still available on materials how can i re-certify the material and use it for the equipment which has the code of construction ASME 2021 .


Regards
Saurabh Joshi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3f6c2884-c436-4ef3-9905-5e2c51713a72n%40googlegroups.com.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0cf8e0a5-a2c7-4cfb-a84f-50604b8a6054n%40googlegroups.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...