Re: [MW:33550] HEAT EXCHANGER CONSTRUCTION


Sir ji 

I too concerned  about DSS cladding including   DSS HEX tubes .
Is it ?

Vishwas 

On Thursday, October 6, 2022 at 10:00:03 AM UTC+5:30 MW wrote:
Does the tube sheet have a lip? Please share a sketch at the weld location? practically it is difficult to avoid heat exposure to duplex clad? you need to change clad material, check with your process metallurgist

On Thu, 6 Oct 2022 at 09:52, Vishwas Keskar Welding Manager WELDING <vvkes...@gmail.com> wrote:
Dear Experts 
One of HEX involves  following MOCs -
HEX tubes - SA 789 TYP 32205 
Tubesheet -SA 266 CL 2 CS - Tube sheet IS cladded with TYP S32205  overlay.
Shell side - CS -SA 516 GR 70 - 75mm thk 
Channel side - CS- SA 516 GR 70 - 75 mm thk 
PWHT is required for  Tube sheet to Shell welding and Tube sheet to Channel welding. These are butt welds with CS Weld metal .
PWHT is not required for  Tube sheet to HEX Tube  welding due to DSS tube to DSS cladding.

Pl advice for the  care that shall be taken during PWHT  of Tube sheet to Shell welding and Tube sheet to Channel welding.

Thanks and regards
Vishwas - IWE
International Welding Engineer


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/709cb8f5-63d1-437a-ba89-6b9c0ba7161bn%40googlegroups.com.

Comments

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...