Re: [MW:30696] Procedure qualification


What is your code of construction?
On Mon, 6 Apr 2020 at 15:30, chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,
A welding procedure is qualified with multiple PQRs as below
  1. 3.05mm
  2. 4.19mm
  3. 6.0mm
  4. 25.0mm
With impact requirement.
Now what is the thickness range qualified.

Thanks and regards,
Venkatramulu CH

-

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubnGDeWs4PbO%2Bm57fNKKpYgi3g9WzCUPqVZrfT8naQ%3Dizg%40mail.gmail.com.

No comments:

[MW:35692]