Re: [MW:30776] Run-Out Length for SMAW Process

Sir how we can find heat input in manual method. It's formulae 

On Thu, Apr 16, 2020, 17:37 Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Dindo, this is not formula for runout length, it is alternative method to find out Heat input. Generally, for Manual welding process, to find out Heat input, it is always better to use run out length method. 

On Thu, 16 Apr 2020 8:56 am Dindo, <dindodelacruz@gmail.com> wrote:
QW-409.1 (a) - ASME Section IX

On Wed, Apr 15, 2020 at 12:28 AM harenath jha <harenathjha@gmail.com> wrote:
From which refrence this formulae has been taken??

On Wed, Apr 15, 2020, 09:19 Dindo <dindodelacruz@gmail.com> wrote:
Run out length is the S in below formula, it is the length of the weld (mm or inches) with the corresponding time to do that length of weld (seconds or minutes)




On Mon, Apr 13, 2020 at 11:08 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Volume of weld metal deposited per burnt length of each Electrode. ISO 1101-1,2 maybe referred also

On Tue, 14 Apr 2020 9:38 am 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
I am not sure with the below mails but I can give explanation to Run-out Length.

In SMAW process, the distance welded by a single electrode (350/450mm length) and it is related to welding speed

Thanks & Regards

J.Gerald Jayakumar




On Monday, April 13, 2020, 07:17:45 PM GMT+7, Vishwas Keskar Welding Manager Pune India <vvkeskar123@gmail.com> wrote:


PL. EXPLAIN MORE 

What is this ?

> 100 mm is min 150 mm
< 100 mm is min 100 mm

Or you can apply simple logic:

Thickness of base metal / each layer height = No of layers * 10-20  mm (staggering length at each layer depending upon the process)



On Sunday, April 10, 2016 at 8:25:07 PM UTC+4, Maulik H. Thakkar wrote:

Dear sir,

Recommended run in run out length for base metal thickness;
> 100 mm is min 150 mm
< 100 mm is min 100 mm

Or you can apply simple logic:

Thickness of base metal / each layer height = No of layers * 10-20  mm (staggering length at each layer depending upon the process)

Regards,
Maulik

On Apr 10, 2016 2:25 PM, "Kurniatullah Sirajudin" <kurniatull...@gmail. com> wrote:
Dear Expert,

A week ago, i received comment regarding welding for smaw process.

My client ask to me, run-out length for smaw process.

I don't know what is run-out length.


Please advise me 


Thank you & Regards

Kurniatullah Sirajudin

--
http://www.linkedin.com/ groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ bb9ef69c-8c36-42e8-b090- 7dd6d32d8af3%40googlegroups. com.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e21dba0d-3601-4908-a012-deccee00c495%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1864291333.3272837.1586791670646%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePpOTnGYxhLCX8OVoSKNE%2BQCyo57fgm-_-NeqwcdCNBOQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGta9%3Dt8KcU-E2a4-LwO7NONBD2tGZmHESYAkcU63b0dWLiMGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOarJYCW3W_ueJBCNt3Ec5x2oXroKdk8iwDTLt89GtfKA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGta9%3DsjF-SDt8YW0_Evjw%3DmVqBp-jf%3DbOsPCrYWQn8at2BmoQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMWcYeGxo6LkTZ8jpG%3DwRjcjfAOkbrhLz6NoEKcNcG18Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UNedgYbkQZLcWPrnTpxwoX%2Bf3BeMwhzjEpnkrSahU_KUQ%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...