Monday, April 6, 2020

Re: [MW:30697] Procedure qualification

Yes

With best regards,
Venkatramulu CH

On Mon, Apr 6, 2020 at 3:35 PM Charles Jacob <charlesvj@gmail.com> wrote:
Hi dear,  are you using b31.3 as the construction code. 

Pl clarify, 

Regards, 

Charles  V Jacob 
 

On Mon, Apr 6, 2020, 2:00 PM chiluka venkatramulu <ramuluchiluka@gmail.com> wrote:
Dear All,
A welding procedure is qualified with multiple PQRs as below
  1. 3.05mm
  2. 4.19mm
  3. 6.0mm
  4. 25.0mm
With impact requirement.
Now what is the thickness range qualified.

Thanks and regards,
Venkatramulu CH

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdFJX%2B%2B8s4ZU0fCuGeWcGfih9rH_D7EUxJv4hZjPohLgvg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKpzM4Bx4U0Eqy3o1PvdSd7u2H_NazQLHxcrSO4Dy4msO1CNUw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdGsOA4kjthWEd_XZ-HeZ8LRLoVtjn1r1KxyYk0gZf8ZtA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...