Re: [MW:29540] Re: ASME Sec-IX ( QW-403.5) interpretation

Yes.It qualifies the listed all three base materials using same F.No.as used for qualification.

On Sun, Apr 28, 2019 at 6:51 PM Souravbohray <ermechsouravbohray@gmail.com> wrote:
1.p number is essential variable  either impact required or not .
2.g number is essential impact required 
3.f and a number is essential  either impact required or not
so we can only weld P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1
CORRECT ME IF I AM WRONG

On Monday, 24 August 2009 09:27:51 UTC+5:30, Kural wrote:
Interpretation: Answer is yes ( for all 3 combination of basemetals) as long as other essential and supplemtary essential are unchanged.
 


 
On Sun, Aug 23, 2009 at 9:48 PM, Sukamal Naskar <sukama...@gmail.com> wrote:
Dear All,
Good Morning !!!
 
I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )
 

QW-403.5 (c ) , states that " ---------------   In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified."

 

Query: If we qualify one PQR, with P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1 material using  SMAW ( E 309MoL) process with impact testing  on weld metal & both HAZ portion , does this PQR supports the following WPS combination of base metals , if all other welding variables are unchanged ?

 

(i)                  P-No. 1 Gr.No.2  to  P-No. 1 Gr.No.2 

(ii)                P-No. 1 Gr.No.2  to  P-No. 8 Gr.No.1 

(iii)               P-No. 8 Gr.No.1  to  P-No. 8 Gr.No.1 

 

Please give your comments,

 

Thanking you,

Regards,
--
Sukamal Naskar
Malaysia





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .