What is your joint configuration ? what is the purpose ?
Regards,
Johnson Prabu
On Saturday 9 December 2017, 10:31:47 AM GMT+3, Sathish Kumar <sathishmech04@gmail.com> wrote:
Dear All
Thanks for the feedback.
I have tried with fillerwire ER4043 also in trial basis. But same problem we have facing.
Wrap around bend test 16T is followed for bend test. Ultra high purity argon used for welding. Spray transfer mode is followed with current 190-220 Amps, Volt 22-24, HI- 0.9KJ/mm with no weaving.
But facing same problem. Any other inputs need to be added, kindly Clarify
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Thanks for the feedback.
I have tried with fillerwire ER4043 also in trial basis. But same problem we have facing.
Wrap around bend test 16T is followed for bend test. Ultra high purity argon used for welding. Spray transfer mode is followed with current 190-220 Amps, Volt 22-24, HI- 0.9KJ/mm with no weaving.
But facing same problem. Any other inputs need to be added, kindly Clarify
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.