Re: [MW:27243] tack weld on the bevel

If you use Good Welder for Tack Weld then you can make tack weld in the bevel and incorporate the Tack weld in Final weld  or else it is advisable to use Bridge Tacks

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On ‎Sunday‎, ‎December‎ ‎31‎, ‎2017‎ ‎12‎:‎14‎:‎08‎ ‎PM‎ ‎IST, 44897 <malgireddy.2007@gmail.com> wrote:


Dear experts,

Can we allow tack weld on the bevel face during fit up or
we need to weld base metal to base metal.

Best regards


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...