hi dear sir 


please be informed that as per API 5L STD. 
 The tolerances for straightness shall be as follows.
a) The total deviation from a straight line, over the entire pipe length, shall be ≤ 0,2 % of the pipe length,

b) The local deviation from a straight line in the 1,0 m (3.0 ft) portion at each pipe end shall be
≤ 4,0 mm (0.156 in).


 best regards
`h.sarpasi
On Wednesday, December 13, 2017, 10:45:41 AM GMT+3:30, Rajendra Jadhav <raj04aug@gmail.com> wrote:


Dear Sir,


Pls provide me the Straightness Criteria for APL 5L X52M.

waiting for replay.

Regards,
Rajendra Jadhav

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...