Where s the location of fracture...?
-- HAZ...?
share photos if possible.
On Sun, Dec 10, 2017 at 9:39 AM, Hani Al Masry <hanyonalfy@gmail.com> wrote:
change to ER 5356Series 6 is heat treatable however small preheat only are required for your caseRegards,H,A--On Sat, Dec 9, 2017 at 11:06 AM, Sathish Kumar <sathishmech04@gmail.com> wrote:Dear All
Thanks for the feedback.
I have tried with fillerwire ER4043 also in trial basis. But same problem we have facing.
Wrap around bend test 16T is followed for bend test. Ultra high purity argon used for welding. Spray transfer mode is followed with current 190-220 Amps, Volt 22-24, HI- 0.9KJ/mm with no weaving.
But facing same problem. Any other inputs need to be added, kindly Clarify
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments