dear sir 
hi
 please be informed that as per ASME B31.8 reduction or 10 percent of thickness is accepted and no need for repair but if you insist for repair this solution is acceptable and you can repair the area by low hydrogen electrode E7018 size 2.4mm(baking and using as per manufacturer recommendation).meanwhile you can repair the area by composite without PWHT.
best regards
h.sarpasi
                                                      On Saturday, December 9, 2017, 6:06:09 AM GMT+3:30, 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com> wrote:                      
                      We have a feed water piping ( A 106  C ) thickness is 47 mm we remark a thickness lost of 3.5 to 4 mm( during supports modification ).
Our construction team propose to repair this damage by welding ( the same WPS used for production ) and after PWHT and NDE .
According your experience this solution it's acceptable or we should cut the damaged area and replace by new spool ?
regards
SALHI Raouf
QA/QC Engineer
Tel: Morocco +212628979891
      Tunisia +21621458258
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments