Dear sir,
Please verify gas purity, I guess higher impurities added with carbon makes cracking.
Thanks & Regards
DINESH VITTHAL SOMWANSHI
BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi
ą¤ ą¤øą„ ą¤¦ą„ą¤Æą¤¾ą¤µą„ दया ą¤¤ą„ą¤®ą¤ą„या ą¤²ą¤¾ą¤ą¤¤ą¤øą„ पाया.
*Pray for others, sometime, You might never need to pray for yourself
again.....*
BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi
ą¤ ą¤øą„ ą¤¦ą„ą¤Æą¤¾ą¤µą„ दया ą¤¤ą„ą¤®ą¤ą„या ą¤²ą¤¾ą¤ą¤¤ą¤øą„ पाया.
*Pray for others, sometime, You might never need to pray for yourself
again.....*
On Fri, Dec 8, 2017 at 11:03 PM, krishnan T <krishrev@gmail.com> wrote:
In my opinion No preheating, Aluminum oxide will form,breaking may be the reason . Try without preheating.--On 08-Dec-2017 4:09 PM, "Sathish Kumar" <sathishmech04@gmail.com> wrote:Dear Experts
I need query on Aluminium welding
Material -6061-T6
Material Thickness-16mm
Filler wire- ER4046
Process-GMAW
Pre heat-70 centigrade
Interpass- 120 centigrade
Preclean by Acetone cleaner and SS wire brush
Gas-Ulta high purity Argon gas
During PQR qualifications we face failure in bend test. Crack open at 30degree itself. Is the above method required PWHT after welding. If so what is the method of PWHT and cycle.
Kindly clarify?
Thanks in advance
Regards
Sathish
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments