hi
can anyone know what is the range of qualification for 40mm thk plate (QW-403.8) for FCAW process. because QW-451 note-3 not shows FCAW process so confused. whether 2T or 5-200mm

On Sunday, 11 October 2009 10:53:27 UTC+5:30, Shashank Vagal wrote:
Hi Group Members,
Please see the following and advise.
Shashank Vagal

Query:

dear every one,

i have this problem i need to know the thickness range or pipes diameter range for the wps in which standard i think its in asme sec 9 but where ???

for exmple if i have wps for thickness 15 is it cover the 20 mm

waiting answer please

regards


My Reply:

 

A WPS is a guideline to ensure joint integrity as proven by PQR + applicable mech tests + NDT. It is intended for all job sizes once the welding technique used proves itself in these tests. The sizes etc come in to picture by qualifying welder on test coupons of a given size as per your job requirements. ASME IX stipulates weld metal deposit and not job size. Please ref to QW 450 - 461.




Now, send attachments up to 25MB with Yahoo! India Mail. Learn how.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...