Wednesday, December 13, 2017

[MW:27188] MR0103 Marking required or LOC . Which one acceptable

Dear Sir,

Material: ASTM 182 Gr 321H (FLANGE)
Size:1/2 inch x sch 80 s

As per client requirement MR0103
Manufacture not marking on flange as MR0103 , But manufacture given LOC for flange as meeting requirement MR0103.
 In MR0103 did not mentioned formarking,but MR0175 they mentioned at para 7.1 marking or documents also acceptable.

1)Is it acceptable or not.
2) according to which standard.

Please give advice and solution.

Regards
ASN


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...