Wednesday, December 13, 2017

[MW:27176] RE: 27169] Welder Qualification for E & I work

This is not a pressure vessel or any critical structure for opting of WQT.

However as a quality engineer we should ensure the ability / performance of the welder.

Hence any of the code provisions or earlier experience certification is sufficient as per my perspective.

As per ASME 3G and above qualified welder is suitable for this application (on plate also sufficient)

 

Else if any client specific norms are defined for this application than we have to extract the client spec, and their expectations and their norms. (viz ASME, AWS, IS Etc)

 

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pavan kumar reddy Juturu
Sent: Tuesday, December 12, 2017 9:52 PM
To: materials-welding@googlegroups.com
Subject: [MW:27169] Welder Qualification for E & I work

 

Dear Experts, 

 

Kindly give your suggestion that in which position WQT should carry out Electrical and instrumentation cable tray and supports welding work, and what should the size of test piece.

 

Thanking you,

 

Pavan.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...