[MW:27144] HOW TO DECIDE NUMBER OF WELDING PASSES REQUIRED TO BE WELDED BASED ON THICKNESS OF BASE PLATE? OR FOR DIFFERENT PLATE THICKNESS

welding throat for two diff thickness is .7 x min thickness of plate.
for same thickness throat should be more than thickness of plates.

--