Saturday, February 13, 2016

Re: [MW:24284] welding of Slip on flange to Pipe

See app. 2 of Div 2

Sent from my BlackBerry 10 smartphone.
From: DHANUSH PR
Sent: Σάββατο, 13 Φεβρουαρίου 2016 - 11:37
To: Materials & Welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24277] welding of Slip on flange to Pipe

Hello Welding Experts

Attached here with a drawing of Slip on flange welding with a Pipe. As per ASME B 31.1/ASME Sec VIII Dev 1 what is acceptable value of 'y' i.e. distance between raised face flange and weld on pipe.


Regards


Dhanush P R


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9113b938-df01-4973-8582-f1eb9b8729b0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...